ప్లాటినం, 00Pt |
|
Pronunciation | (PLAT-ən-əm) |
---|
Appearance | grayish white |
---|
|
|
| |
---|
|
|
|
Group | మూస:Infobox element/symbol-to-group/format |
---|
Period | period 6 |
---|
Block | d-block |
---|
Electron configuration | [Xe] 4f14 5d9 6s1 |
---|
Electrons per shell | 2, 8, 18, 32, 17, 1 |
---|
|
Phase at STP | solid |
---|
Melting point | 2041.4 K (1768.3 °C, 3214.9 °F) |
---|
Boiling point | 4098 K (3825 °C, 6917 °F) |
---|
Density (near r.t.) | 21.45 g/cm3 |
---|
when liquid (at m.p.) | 19.77 g/cm3 |
---|
Heat of fusion | 22.17 kJ/mol |
---|
Heat of vaporization | 469 kJ/mol |
---|
Molar heat capacity | 25.86 J/(mol·K) |
---|
Vapor pressure
P (Pa)
|
1
|
10
|
100
|
1 k
|
10 k
|
100 k
|
at T (K)
|
2330
|
(2550)
|
2815
|
3143
|
3556
|
4094
|
|
|
Oxidation states | −3, −2, −1, 0, +1, +2, +3, +4, +5, +6 (a mildly basic oxide) |
---|
Electronegativity | Pauling scale: 2.28 |
---|
Atomic radius | empirical: 139 pm |
---|
Covalent radius | 136±5 pm |
---|
Van der Waals radius | 175 pm |
---|
Spectral lines of ప్లాటినం |
|
Natural occurrence | primordial |
---|
Crystal structure | face-centered cubic (fcc) |
---|
Speed of sound thin rod | 2800 m/s (at r.t.) |
---|
Thermal expansion | 8.8 µm/(m⋅K) (at 25 °C) |
---|
Thermal conductivity | 71.6 W/(m⋅K) |
---|
Electrical resistivity | 105 n Ω⋅m (at 20 °C) |
---|
Magnetic ordering | paramagnetic |
---|
Young's modulus | 168 GPa |
---|
Shear modulus | 61 GPa |
---|
Bulk modulus | 230 GPa |
---|
Poisson ratio | 0.38 |
---|
Mohs hardness | 4–4.5 |
---|
Vickers hardness | 549 MPa |
---|
Brinell hardness | 392 MPa |
---|
CAS Number | 7440-06-4 |
---|
|
Discovery | Antonio de Ulloa (1735) |
---|
First isolation | Antonio de Ulloa (1735) |
---|
|
Template:infobox ప్లాటినం isotopes does not exist |
Category: ప్లాటినం | references |
References
These references will appear in the article, but this list appears only on this page.